Stoneware V9G
Method: Throwing, modelling
The addition of grogg gives good resistance to cracking and warping. V9G behaves well under oxidising and reduction conditions.
Firing Range: 1120°C – 1280°C
Bag Size: 12.5kg
Method: Throwing, modelling
The addition of grogg gives good resistance to cracking and warping. V9G behaves well under oxidising and reduction conditions.
Firing Range: 1120°C – 1280°C